Polymer Property : Maximum Service Temperature, Inert = 1650 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 1650 °C
3000 °F
Aremco Ceramabind™ 542 High Temperature Inorganic Binder
Single part, low viscosity, water-dispersed, aluminum phosphate solution for penetrating ultra fine thermal spray applications to 3000°F (1650°C).