Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | -70.0 °C | -94.0 °F | |
DuPont Teijin Films Mylar® M461 Polyester Film, 142 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Maximum Service Temperature, Inert | -70.0 °C | -94.0 °F | |
DuPont Teijin Films Mylar® M461 Polyester Film, 200 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Maximum Service Temperature, Inert | -70.0 °C | -94.0 °F | |
DuPont Teijin Films Mylar® M461 Polyester Film, 48 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Maximum Service Temperature, Inert | -70.0 °C | -94.0 °F | |
DuPont Teijin Films Mylar® M461 Polyester Film, 500 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Maximum Service Temperature, Inert | -70.0 °C | -94.0 °F | |
DuPont Teijin Films Mylar® M461 Polyester Film, 60 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Maximum Service Temperature, Inert | -70.0 °C | -94.0 °F | |
DuPont Teijin Films Mylar® M461 Polyester Film, 75 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Maximum Service Temperature, Inert | -70.0 °C | -94.0 °F | |
DuPont Teijin Films Mylar® M461 Polyester Film, 92 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Maximum Service Temperature, Inert | -70.0 °C | -94.0 °F | |
DuPont Teijin Films Mylar® M577 Polyester Film, 48 Gauge Mylar® Type M577 is a tough, transparent film. A rough surface provides ease of handling, good adhesion, and processability.General Product Info: Mylar® Type M577 film has balanced tensile propert.. |
|||
Maximum Service Temperature, Inert | -70.0 °C | -94.0 °F | |
DuPont Teijin Films Mylar® S1 Polyester Film, 20 Gauge Mylar® S1 films are slightly hazy with surfaces tailored to provide excellent handling and product functionality for a variety of industrial end uses. The outstanding tensile properties and thermal.. |
|||
Maximum Service Temperature, Inert | -70.0 °C | -94.0 °F | |
DuPont Teijin Films Mylar® S1 Polyester Film, 25 Gauge Mylar® S1 films are slightly hazy with surfaces tailored to provide excellent handling and product functionality for a variety of industrial end uses. The outstanding tensile properties and thermal.. |
|||
Maximum Service Temperature, Inert | -70.0 °C | -94.0 °F | |
DuPont Teijin Films Mylar® S1 Polyester Film, 35 Gauge Mylar® S1 films are slightly hazy with surfaces tailored to provide excellent handling and product functionality for a variety of industrial end uses. The outstanding tensile properties and thermal.. |
|||
Maximum Service Temperature, Inert | -70.0 °C | -94.0 °F | |
DuPont Teijin Films Mylar® M461 Polyester Film, 300 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Maximum Service Temperature, Inert | -70.0 °C | -94.0 °F | |
DuPont Teijin Films Mylar® M461 Polyester Film, 400 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |