Thermal Properties Metric English Comments
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
DuPont Teijin Films Mylar® M461 Polyester Film, 142 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
DuPont Teijin Films Mylar® M461 Polyester Film, 200 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
DuPont Teijin Films Mylar® M461 Polyester Film, 48 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
DuPont Teijin Films Mylar® M461 Polyester Film, 500 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
DuPont Teijin Films Mylar® M461 Polyester Film, 60 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
DuPont Teijin Films Mylar® M461 Polyester Film, 75 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
DuPont Teijin Films Mylar® M461 Polyester Film, 92 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
DuPont Teijin Films Mylar® M577 Polyester Film, 48 Gauge
Mylar® Type M577 is a tough, transparent film. A rough surface provides ease of handling, good adhesion, and processability.General Product Info: Mylar® Type M577 film has balanced tensile propert..
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
DuPont Teijin Films Mylar® S1 Polyester Film, 20 Gauge
Mylar® S1 films are slightly hazy with surfaces tailored to provide excellent handling and product functionality for a variety of industrial end uses. The outstanding tensile properties and thermal..
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
DuPont Teijin Films Mylar® S1 Polyester Film, 25 Gauge
Mylar® S1 films are slightly hazy with surfaces tailored to provide excellent handling and product functionality for a variety of industrial end uses. The outstanding tensile properties and thermal..
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
DuPont Teijin Films Mylar® S1 Polyester Film, 35 Gauge
Mylar® S1 films are slightly hazy with surfaces tailored to provide excellent handling and product functionality for a variety of industrial end uses. The outstanding tensile properties and thermal..
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
DuPont Teijin Films Mylar® M461 Polyester Film, 300 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
DuPont Teijin Films Mylar® M461 Polyester Film, 400 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..