Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 13.6 W/m-K | 94.4 BTU-in/hr-ft²-°F | |
Special Metals INCONEL® Alloy 617 A nickel-chromium-cobalt-molybdenum alloy with an exceptional combination of metallurgical stability, strength, and oxidation resistance at high temperatures. Resistance to oxidation is enhanced by.. |