Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | >= 90.0 W/m-K | >= 625 BTU-in/hr-ft²-°F | |
H.C. Starck HPM 1701 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Thermal Conductivity | 90.0 W/m-K | 625 BTU-in/hr-ft²-°F | |
UCAR Carbon UCAR® ATA Isostatic Molded Graphite Economical grade ATA is the lowest density version of isostatically molded, fine grain grade ATJ family of graphite materials.Typical Applications: ATA is used in general purpose applications where .. |
|||
Thermal Conductivity | 90.0 W/m-K | 625 BTU-in/hr-ft²-°F | |
California Fine Wire Nickel Alloy 60 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Thermal Conductivity | 90.0 W/m-K | 625 BTU-in/hr-ft²-°F | |
AK Steel ASTM A 424 Type 1, UNIVIT® DS Enameling Carbon Steel UNVIT is a specialty enameling steel developed for applications where direct-on cover coat enameling is employed. This product is free of porcelain enamel fishscale regardless of the enameling syst.. |
|||
Thermal Conductivity | 90.0 W/m-K | 625 BTU-in/hr-ft²-°F | |
Ceradyne Ceralloy® 546-3E Boron Carbide Features:low porosityhigh puritysingle phaseApplications:semiconductor componentsInformation provided by Ceradyne Company |
|||
Thermal Conductivity | 90.0 W/m-K | 625 BTU-in/hr-ft²-°F | |
Ceradyne Ceralloy® 546-4E Boron Carbide Features:neutron absorptionwear resistancehardnesslightweightApplications:semiconductor componentswear componentsballistic armorsputtering targetsnuclear shieldingInformation provided by Ceradyne Co.. |
|||
Thermal Conductivity | 90.0 W/m-K | 625 BTU-in/hr-ft²-°F | |
Ceradyne Ceralloy® 546 Boron Carbide Features:neutron absorptionwear resistancehardnesslightweightApplications:semiconductor componentswear componentsballistic armorsputtering targetsnuclear shieldingInformation provided by Ceradyne Co.. |
|||
Thermal Conductivity | 90.0 W/m-K | 625 BTU-in/hr-ft²-°F | |
Ohio Carbon Blank OCB TTK-4 EDM Grade Graphite Available in a range of sizes and shapes. |
|||
Thermal Conductivity | 90.0 W/m-K @Temperature 500 °C |
625 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Plansee DENSIMET® D185 Tungsten-Nickel-Iron Alloy Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d.. |