Polymer Property : Thermal Conductivity = 625 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity >= 90.0 W/m-K
>= 625 BTU-in/hr-ft²-°F
H.C. Starck HPM 1701 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Thermal Conductivity 90.0 W/m-K
625 BTU-in/hr-ft²-°F
UCAR Carbon UCAR® ATA Isostatic Molded Graphite
Economical grade ATA is the lowest density version of isostatically molded, fine grain grade ATJ family of graphite materials.Typical Applications: ATA is used in general purpose applications where ..
Thermal Conductivity 90.0 W/m-K
625 BTU-in/hr-ft²-°F
California Fine Wire Nickel Alloy 60 Copper Nickel Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Thermal Conductivity 90.0 W/m-K
625 BTU-in/hr-ft²-°F
AK Steel ASTM A 424 Type 1, UNIVIT® DS Enameling Carbon Steel
UNVIT is a specialty enameling steel developed for applications where direct-on cover coat enameling is employed. This product is free of porcelain enamel fishscale regardless of the enameling syst..
Thermal Conductivity 90.0 W/m-K
625 BTU-in/hr-ft²-°F
Ceradyne Ceralloy® 546-3E Boron Carbide
Features:low porosityhigh puritysingle phaseApplications:semiconductor componentsInformation provided by Ceradyne Company
Thermal Conductivity 90.0 W/m-K
625 BTU-in/hr-ft²-°F
Ceradyne Ceralloy® 546-4E Boron Carbide
Features:neutron absorptionwear resistancehardnesslightweightApplications:semiconductor componentswear componentsballistic armorsputtering targetsnuclear shieldingInformation provided by Ceradyne Co..
Thermal Conductivity 90.0 W/m-K
625 BTU-in/hr-ft²-°F
Ceradyne Ceralloy® 546 Boron Carbide
Features:neutron absorptionwear resistancehardnesslightweightApplications:semiconductor componentswear componentsballistic armorsputtering targetsnuclear shieldingInformation provided by Ceradyne Co..
Thermal Conductivity 90.0 W/m-K
625 BTU-in/hr-ft²-°F
Ohio Carbon Blank OCB TTK-4 EDM Grade Graphite
Available in a range of sizes and shapes.
Thermal Conductivity 90.0 W/m-K

@Temperature 500 °C
625 BTU-in/hr-ft²-°F

@Temperature 932 °F
Plansee DENSIMET® D185 Tungsten-Nickel-Iron Alloy
Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d..