Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.200 - 1.44 W/m-K @Temperature 80.0 - 250 °C |
1.39 - 9.99 BTU-in/hr-ft²-°F @Temperature 176 - 482 °F |
Average value: 0.480 W/m-K Grade Count:18 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |