Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 123 W/m-K | 852 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals UNS C38500 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |