Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.29 W/m-K | 8.95 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® E3001-6 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E3001-HV is a snap cure, single component, silver-filled die attach adhesive for semiconductor plastic IC packaging. Also available in a frozen syringe. Advantages & .. |