Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 8.20 W/m-K @Temperature 800 °C |
56.9 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
McDanel Advanced Ceramics 99.8% Alumina Information provided by McDanel Advanced Ceramic Technologies |