Thermal Properties Metric English Comments
Thermal Conductivity 8.20 W/m-K

@Temperature 800 °C
56.9 BTU-in/hr-ft²-°F

@Temperature 1470 °F
McDanel Advanced Ceramics 99.8% Alumina
Information provided by McDanel Advanced Ceramic Technologies