Thermal Properties Metric English Comments
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
RT
Outokumpu 353MA® High Temperature Austenitic Stainless Steel
Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but..
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
Kennametal Stellite Delcrome® 93
Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Highly alloyed white cast iron, abrasion resistant. Carbides in a martensitic matrix offer high..
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
RT
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
RT
Haynes 242® alloy
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
RT
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
RT
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
RT
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
RT
Haynes 242® alloy, cold reduced sheet, annealed
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
RT
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
RT
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
RT
Haynes 242® alloy, cold reduced sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
RT
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
Special Metals NIMONIC® Alloy PK33
A nickel-chromium-cobalt alloy that is precipitation hardenable and also contains a relatively high (7%) level of molybdenum for solid-solution strengthening. It has an exceptional combination of h..
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
California Fine Wire Stablohm 650 Nickel Chromium Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.