Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 95.0 - 105 W/m-K | 659 - 729 BTU-in/hr-ft²-°F | |
Ceradyne Ceralloy® 137 CB AlN Composite Applications: replacement for Ceralloy® 2710 BeO-SiCterminationssever wedgesload pelletsabsorbersFeatures: higher thermal conductivity then Ceraloy® BeO-SiC at temperatures greater then 150°C, cl.. |