Polymer Property : Thermal Conductivity = 105 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 95.0 - 105 W/m-K
659 - 729 BTU-in/hr-ft²-°F
Ceradyne Ceralloy® 137 CB AlN Composite
Applications: replacement for Ceralloy® 2710 BeO-SiCterminationssever wedgesload pelletsabsorbersFeatures: higher thermal conductivity then Ceraloy® BeO-SiC at temperatures greater then 150°C, cl..