Thermal Properties Metric English Comments
Thermal Conductivity 9.50 W/m-K
65.9 BTU-in/hr-ft²-°F
Longitudinal
LATI Laticonther 82 CP1/800 PA12
High thermal conductivity product based on Polyamide 12 (PA12). Special fillerAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..