Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 79.3 W/m-K | 550 BTU-in/hr-ft²-°F | |
Special Metals Nickel 201 Commercially pure (99.6%) wrought nickel essentially the same as Nickel 200 but with a lower carbon content to prevent embrittlement by intergranular carbon at temperatures over 600°F (315°C)... |