Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Special Metals Nickel 201

Category Metal , Nonferrous Metal , Nickel Alloy , Pure Element
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals Nickel 201.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Commercially pure (99.6%) wrought nickel essentially the same as Nickel 200 but with a lower carbon content to prevent embrittlement by intergranular carbon at temperatures over 600°F (315°C). Lower carbon content also reduces hardness, making Nickel 201 particularly suitable for cold-formed items. Ferromagnetic. Standard product forms are round, flats, pipe, tube, plate, sheet, forging stock, strip, and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 403 MPa
58500 psi
Annealed
350 MPa

@Temperature 300 °C
50800 psi

@Temperature 572 °F
Annealed prior to test
Tensile Strength, Yield 103 MPa
14900 psi
Annealed
95.0 MPa

@Temperature 300 °C
13800 psi

@Temperature 572 °F
Annealed prior to test
Elongation at Break 50 %
50 %
Annealed prior to test.
41 %

@Temperature 300 °C
41 %

@Temperature 572 °F
Annealed prior to test.
Thermal Properties Metric English Comments
CTE, linear 13.1 µm/m-°C

@Temperature 20.0 - 100 °C
7.28 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.456 J/g-°C
0.109 BTU/lb-°F
Thermal Conductivity 79.3 W/m-K
550 BTU-in/hr-ft²-°F
Melting Point 1435 - 1446 °C
2615 - 2635 °F
Solidus 1435 °C
2615 °F
Liquidus 1446 °C
2635 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.020 %
<= 0.020 %
Copper, Cu <= 0.25 %
<= 0.25 %
Iron, Fe <= 0.40 %
<= 0.40 %
Manganese, Mn <= 0.35 %
<= 0.35 %
Nickel, Ni >= 99 %
>= 99 %
Including Cobalt
Silicon, Si <= 0.35 %
<= 0.35 %
Sulfur, S <= 0.010 %
<= 0.010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000850 ohm-cm
0.00000850 ohm-cm
Curie Temperature 360 °C
680 °F
Copyright © lookpolymers.com All Rights Reserved