Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.803 W/m-K
5.57 BTU-in/hr-ft²-°F
ASTM C177
Devcon Brushable Ceramic - Red, Blue Epoxy
Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,..
Thermal Conductivity 0.803 W/m-K
5.57 BTU-in/hr-ft²-°F
ASTM C177
Devcon Brushable Ceramic - White Epoxy
Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,..
Thermal Conductivity 0.803 W/m-K
5.57 BTU-in/hr-ft²-°F
ASTM C177
Devcon Sprayable Ceramic™ Epoxy
Precision Repair EpoxyComments: A sprayable ceramic-reinforced composite that can be sprayed in a manner similar to high-solid paints. Ideal for protecting pumps, paper machines, stacks, pump pads,..