Thermal Conductivity 0.600 - 0.800 W/m-K
4.16 - 5.55 BTU-in/hr-ft²-°F
ASTM E1461
Raschig Group 3505 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
Thermal Conductivity 0.600 - 0.800 W/m-K
4.16 - 5.55 BTU-in/hr-ft²-°F
ASTM E1461
Raschig Group 3535 Epoxy
Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack..
Thermal Conductivity 0.590 - 0.800 W/m-K
4.09 - 5.55 BTU-in/hr-ft²-°F
Average value: 0.643 W/m-K Grade Count:6
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min..
Thermal Conductivity 0.277 - 0.800 W/m-K
1.92 - 5.55 BTU-in/hr-ft²-°F
Average value: 0.540 W/m-K Grade Count:16
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..