Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.586 - 0.795 W/m-K | 4.06 - 5.51 BTU-in/hr-ft²-°F | |
Abatron AboCast/AboCure 8501-4/8501-4 High Temperature Resistant Epoxy Gray, high viscosity, structural/machinable epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components to be us.. |
|||
Thermal Conductivity | 0.586 - 0.795 W/m-K | 4.06 - 5.51 BTU-in/hr-ft²-°F | |
Abatron AboCast/AboCure 8501-5/8501-4 High Temperature Resistant Epoxy Gray, high viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components to be us.. |