Polymer Property : Thermal Conductivity = 5.40 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.778 W/m-K
5.40 BTU-in/hr-ft²-°F
Saint-Gobain Rulon® II Bearing/Seal PTFE
An injection moldable bearing material that possesses excellent chemical and wear resistance. Rulon II is available in injection molded finished parts only. Excellent friction and wear properties al..