Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.778 W/m-K | 5.40 BTU-in/hr-ft²-°F | |
Saint-Gobain Rulon® II Bearing/Seal PTFE An injection moldable bearing material that possesses excellent chemical and wear resistance. Rulon II is available in injection molded finished parts only. Excellent friction and wear properties al.. |