Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.735 W/m-K | 5.10 BTU-in/hr-ft²-°F | |
Schott SF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.735 W/m-K @Temperature 538 °C |
5.10 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek Pyrocast ZS Refractory Shapes Aggregate Base: Fused SilicaApplicationsTransfer troughs Information provided by Pyrotek. |