Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schott SF2 Glass

Category Ceramic , Glass
Manufacturer Schott North America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott SF2 Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by SCHOTT North America, Inc.
Physical Properties Metric English Comments
Density 3.86 g/cc
0.139 lb/in³
Mechanical Properties Metric English Comments
Knoop Microhardness 410
410
.1/20
Modulus of Elasticity 55.0 GPa
7980 ksi
Poissons Ratio 0.227
0.227
Shear Modulus 22.0 GPa
3190 ksi
calculated
Thermal Properties Metric English Comments
CTE, linear 8.40 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.67 µin/in-°F

@Temperature -22.0 - 158 °F
9.20 µm/m-°C

@Temperature 20.0 - 300 °C
5.11 µin/in-°F

@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.498 J/g-°C
0.119 BTU/lb-°F
Thermal Conductivity 0.735 W/m-K
5.10 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 441 °C
826 °F
Optical Properties Metric English Comments
Refractive Index 1.64769

@Wavelength 587.6 nm
1.64769

@Wavelength 587.6 nm
n<sub>d</sub>
1.65222

@Wavelength 546.1 nm
1.65222

@Wavelength 546.1 nm
n<sub>e</sub>
Transmission, Visible 94.6 %

@Thickness 10.0 mm,
Wavelength 380 nm
94.6 %

@Thickness 0.394 in,
Wavelength 380 nm
98.5 %

@Thickness 10.0 mm,
Wavelength 405 nm
98.5 %

@Thickness 0.394 in,
Wavelength 405 nm
99.5 %

@Thickness 10.0 mm,
Wavelength 460 nm
99.5 %

@Thickness 0.394 in,
Wavelength 460 nm
99.8 %

@Thickness 10.0 mm,
Wavelength 580 nm
99.8 %

@Thickness 0.394 in,
Wavelength 580 nm
99.8 %

@Thickness 10.0 mm,
Wavelength 700 nm
99.8 %

@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance 82.6 %

@Thickness 10.0 mm,
Wavelength 2500 nm
82.6 %

@Thickness 0.394 in,
Wavelength 2500 nm
99.4 %

@Thickness 10.0 mm,
Wavelength 1530 nm
99.4 %

@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance 11 %

@Thickness 10.0 mm,
Wavelength 334 nm
11 %

@Thickness 0.394 in,
Wavelength 334 nm
67.2 %

@Thickness 10.0 mm,
Wavelength 350 nm
67.2 %

@Thickness 0.394 in,
Wavelength 350 nm
87.7 %

@Thickness 10.0 mm,
Wavelength 365 nm
87.7 %

@Thickness 0.394 in,
Wavelength 365 nm
91 %

@Thickness 10.0 mm,
Wavelength 370 nm
91 %

@Thickness 0.394 in,
Wavelength 370 nm
Chemical Properties Metric English Comments
Acid Class, SR 2.0
2.0
Alkali Class, AR 2.3
2.3
Stain Resistance Class, FR 0.00
0.00
Descriptive Properties Value Comments
B 0
Climatic Resistance Test CR 1
HG 2
K (10-6mm2/N) 2.62
Phosphate Resistance PR 2
T1013.0 (°C) 428
T107.6 (°C) 600