Polymer Property : Thermal Conductivity = 5.04 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 5.04 W/m-K
35.0 BTU-in/hr-ft²-°F
Cotronics Duralco™ 134 500°F (260°C) Aluminum Filled Epoxy
Thermally conductive grease provides a non-hardening, electrically insulating and thermally conductive layer between components and heat sinks. Ceramic fillers provide high thermal conductivity alo..
Thermal Conductivity 5.04 W/m-K
35.0 BTU-in/hr-ft²-°F
Cotronics Duralco™ 4540 Machinable Epoxy
Patches, fills, seals, and repairs with outstanding adhesion, ductility, thermal conductivity and shock resistance.Corrosion Resistance: excellent resistance to chemicals and solventsApplications: ..
Thermal Conductivity 5.04 W/m-K
35.0 BTU-in/hr-ft²-°F
Cotronics 454B Machinable Non-Sag Putty Adhesive