Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 49.3 W/m-K | 342 BTU-in/hr-ft²-°F | |
California Fine Wire Nickel 211 (Nickel Manganese Alloy) All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |