Thermal Conductivity 49.3 W/m-K
342 BTU-in/hr-ft²-°F
California Fine Wire Nickel 211 (Nickel Manganese Alloy)
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.