Thermal Properties Metric English Comments
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 Hard, 1.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 1.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 MH10, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 MH12, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 MH6, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 MH8, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H925 (H925) Temper; All Sizes (UNS N03360)
Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.7Formability Ratio (bad Way)..
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard, 1.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 1.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): ..
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard, 2.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 Annealed
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): ..
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 Annealed, 2.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 Hard
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1.2Formability Ratio (bad Way)..
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 MH2, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Beryllium Nickel Strip - Alloy 360 MH4, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Thermal Conductivity 48.0 W/m-K

@Temperature 85.0 °C
333 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy 116 Tin-Lead Solder Alloy
General purpose solderInformation Provided by Indium Corporation
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; A (A) Temper; All Sizes (UNS N03360)
Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H1050 (H1050) Temper; All Sizes (UNS N03360)
Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Thermal Conductivity 48.0 W/m-K
333 BTU-in/hr-ft²-°F
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H775 (H775) Temper; All Sizes (UNS N03360)
Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.