Thermal Properties Metric English Comments
Thermal Conductivity 45.0 W/m-K
312 BTU-in/hr-ft²-°F
Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance
S-679 is an isostatically pressed graphite material that is treated to provide oxidation resistance at elevated temperatures. This material performs well in glass contact applications where heat an..
Thermal Conductivity 45.0 W/m-K

@Temperature 85.0 °C
312 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® 9 Sn-Pb-In Solder Alloy
General purpose solder in 160° C range with good physical properties.Information provided by the manufacturer, Indium Corporation.
Thermal Conductivity 45.0 W/m-K
312 BTU-in/hr-ft²-°F
ThyssenKrupp XABO® 355 Structural Steel
This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Thermal Conductivity 45.0 W/m-K
312 BTU-in/hr-ft²-°F
ThyssenKrupp XABO® 500 T Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Thermal Conductivity 45.0 W/m-K
312 BTU-in/hr-ft²-°F
ThyssenKrupp XABO® 355 T Structural Steel
This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Thermal Conductivity 45.0 W/m-K
312 BTU-in/hr-ft²-°F
ThyssenKrupp XABO® 500 Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Thermal Conductivity 45.0 W/m-K
312 BTU-in/hr-ft²-°F
Eagle Brass 706 Copper Nickel 10%, 1/2 Hard
706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to..
Thermal Conductivity 45.0 W/m-K
312 BTU-in/hr-ft²-°F
Eagle Brass 706 Copper Nickel 10%, 1/4 Hard
706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to..
Thermal Conductivity 45.0 W/m-K
312 BTU-in/hr-ft²-°F
Eagle Brass 706 Copper Nickel 10%, Annealed
706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to..
Thermal Conductivity 45.0 W/m-K
312 BTU-in/hr-ft²-°F
Eagle Brass 706 Copper Nickel 10%, Extra Hard
706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to..
Thermal Conductivity 45.0 W/m-K
312 BTU-in/hr-ft²-°F
Eagle Brass 706 Copper Nickel 10%, Hard
706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to..
Thermal Conductivity 45.0 W/m-K
312 BTU-in/hr-ft²-°F
Eagle Brass 706 Copper Nickel 10%, Spring
706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to..
Thermal Conductivity 45.0 W/m-K
312 BTU-in/hr-ft²-°F
ThyssenKrupp XABO® 460 Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Thermal Conductivity 45.0 W/m-K
312 BTU-in/hr-ft²-°F
ThyssenKrupp XABO® 460 T Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..