Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 40.0 W/m-K @Temperature 20.0 °C |
278 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel Superplast® SP300 Prehardened Mold Steel Superplast® 300 (SP300) is a prehardened steel with a BHN 300 (32 HRC) to be used for plastic injection molds, extrusion dies, and compression molds offering improved performance for the mold mak.. |
|||
Thermal Conductivity | 40.0 W/m-K | 278 BTU-in/hr-ft²-°F | |
Aremco AREMCOLOX™ 502-1800 Machinable Aluminum Nitride Hot-pressed boron nitride – aluminum nitride composite that demonstrates high thermal conductivity, dielectric strength, and abrasion resistance. Readily machined and available in rods from 1/4” t.. |