Thermal Properties Metric English Comments
Thermal Conductivity 0.330 - 4.00 W/m-K
2.29 - 27.8 BTU-in/hr-ft²-°F
Average value: 0.462 W/m-K Grade Count:60
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..