Polymer Property : Thermal Conductivity = 360 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 51.9 W/m-K
360 BTU-in/hr-ft²-°F
Materion ToughMet® T2 CX 90
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Thermal Conductivity 51.9 W/m-K

@Temperature 10.0 - 232 °C
360 BTU-in/hr-ft²-°F

@Temperature 50.0 - 450 °F
Meehanite HR Heat Resisting Cast Iron
Type HR is a strong, dense iron of high rigidity and excellent resistance to scaling under most conditions. It possesses good load carrying ability. Recommended for service conditions without ther..
Thermal Conductivity 51.9 W/m-K
360 BTU-in/hr-ft²-°F
Latrobe LSSâ„¢ 135M Nitriding Steel (ASTM A355 Class A)
TLS 135M Nitriding Steel is a high-aluminum and chromium modification of AISI 4140 alloy steel. The aluminum addition promotes the formation of aluminum nitride compounds when tools manufactured fr..
Thermal Conductivity 51.9 W/m-K
360 BTU-in/hr-ft²-°F
Latrobe LSSâ„¢ 4142 Alloy Steel (AISI 4142)
TLS 4140 and 4142HT are versatile, alloy steels which are used in variety of tooling and other industrial applications. TLS 4140 is the classic AISI 4140 alloy steel which is sold in the annealed co..
Thermal Conductivity 51.9 W/m-K
360 BTU-in/hr-ft²-°F
Chicago Extruded Metals BioBrass® UNS C63000 Aluminum Bronze
Finished product available as bar,rod, forged, shapes, or tubes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chica..