Chicago Extruded Metals BioBrass® UNS C63000 Aluminum Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer Chicago Extruded Metals (CXM)
Trade Name BioBrass®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chicago Extruded Metals BioBrass® UNS C63000 Aluminum Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Finished product available as bar,rod, forged, shapes, or tubes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 7.58 g/cc
0.274 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 96 - 98
96 - 98
Tensile Strength 621 - 814 MPa
90000 - 118000 psi
Tensile Strength, Yield 345 - 517 MPa
50000 - 75000 psi
Elongation at Break 15 - 20 %
15 - 20 %
Thermal Properties Metric English Comments
Thermal Conductivity 51.9 W/m-K
360 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Aluminum, Al 9.0 - 11 %
9.0 - 11 %
Copper, Cu >= 76.75 %
>= 76.75 %
as balance
Iron, Fe 2.0 - 4.0 %
2.0 - 4.0 %
Manganese, Mn <= 1.5 %
<= 1.5 %
Nickel, Ni 4.0 - 5.5 %
4.0 - 5.5 %
Other, total 0.50 %
0.50 %
Silicon, Si <= 0.25 %
<= 0.25 %
Tin, Sn <= 0.20 %
<= 0.20 %
Zinc, Zn <= 0.30 %
<= 0.30 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000246 ohm-cm
0.0000246 ohm-cm