Thermal Properties Metric English Comments
Thermal Conductivity 51.3 W/m-K
356 BTU-in/hr-ft²-°F
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy
High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining..