Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.280 - 0.519 W/m-K | 1.94 - 3.60 BTU-in/hr-ft²-°F | Average value: 0.447 W/m-K Grade Count:7 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Thermal Conductivity | 0.220 - 0.519 W/m-K | 1.53 - 3.60 BTU-in/hr-ft²-°F | Average value: 0.383 W/m-K Grade Count:26 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |