Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 28.6 W/m-K @Temperature 216 °C |
198 BTU-in/hr-ft²-°F @Temperature 421 °F |
|
Carpenter No. 883® Hot Work Die Steel (Red-Tough) (AISI H13) No. 883 hot work die steel is a 5% chromium hot work tool steel designed particularly for applications requiring extreme toughness combined with good red-hardness. It has given an extra margin of sa.. |