Polymer Property : Thermal Conductivity = 25.8 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 25.8 W/m-K

@Temperature 900 °C
179 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 25.8 W/m-K

@Temperature 900 °C
179 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 242® alloy
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 25.8 W/m-K

@Temperature 900 °C
179 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 25.8 W/m-K

@Temperature 900 °C
179 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 25.8 W/m-K

@Temperature 900 °C
179 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 25.8 W/m-K

@Temperature 900 °C
179 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 242® alloy, cold reduced sheet, annealed
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 25.8 W/m-K

@Temperature 900 °C
179 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 25.8 W/m-K

@Temperature 900 °C
179 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 25.8 W/m-K

@Temperature 900 °C
179 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 242® alloy, cold reduced sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 25.8 W/m-K

@Temperature 300 °C
179 BTU-in/hr-ft²-°F

@Temperature 572 °F
Crucible Steel CPM® 1V® High Alloy Tool Steel
CPM 1V is a medium carbon, high alloy tool steel which exhibits high toughness combined with high heat resistance. It is suited for both hot or cold applications which demand high impact toughness a..
Thermal Conductivity 25.8 W/m-K

@Temperature 95.0 °C
179 BTU-in/hr-ft²-°F

@Temperature 203 °F
Crucible Steel CRUCIBLE A9 Tool Steel
Crucible A9 is an air-hardening tool steel combining some of characteristics of the 5% chromium hot-work grades (such as H13) with the high attainable hardness and compressive yield strength of the ..