Material Notes:
CPM 1V is a medium carbon, high alloy tool steel which exhibits high toughness combined with high heat resistance. It is suited for both hot or cold applications which demand high impact toughness and also require moderate wear resistance.The CPM (Crucible Particle Metallurgy) process produces very homogeneous, high quality steel characterized by superior dimensional stability, grindability, and toughness compared to steels produced by conventional processes.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 7.85 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 187
187
Annealed
Hardness, Rockwell C 57 - 59
57 - 59
Modulus of Elasticity 207 GPa
30000 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 21.88 W/m-K
151.8 BTU-in/hr-ft²-°F
23.88 W/m-K

@Temperature 100 °C
165.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
25.8 W/m-K

@Temperature 300 °C
179 BTU-in/hr-ft²-°F

@Temperature 572 °F
26.76 W/m-K

@Temperature 400 °C
185.7 BTU-in/hr-ft²-°F

@Temperature 752 °F
28.09 W/m-K

@Temperature 540 °C
194.9 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Component Elements Properties Metric English Comments
Carbon, C 0.55 %
0.55 %
Chromium, Cr 4.5 %
4.5 %
Iron, Fe 89.05 %
89.05 %
As Remainder
Molybdenum, Mo 2.75 %
2.75 %
Tungsten, W 2.15 %
2.15 %
Vanadium, V 1.0 %
1.0 %