Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 25.1 W/m-K | 174 BTU-in/hr-ft²-°F | |
Misumi G-STAR Martensite Free-cutting Stainless Steel Corrosion resistant; excellent machinability. Comparable in material properties and chemical make up to STAVAX mold steel.Information provided by MISUMI Corporation. |
|||
Thermal Conductivity | 25.1 W/m-K @Temperature 20.0 °C |
174 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Schmolz + Bickenbach 416RS Stainless Steel Bar Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc.. |
|||
Thermal Conductivity | 25.1 W/m-K @Temperature 100 °C |
174 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Crucible Steel 422 Stainless Steel Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is.. |
|||
Thermal Conductivity | 25.1 W/m-K | 174 BTU-in/hr-ft²-°F | hardened to 45 HRC |
Bohler-Uddeholm ORVAR® 2M / AISI H13 Hot Work Tool Steel Orvar 2 Microdized is a chromium-molybdenum-vanadium alloyed steelORVAR® 2M / AISI H13 is a conventionally produced hot work tool steel with overall good ductility, toughness, wear resistance, hard.. |