Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 224 - 240 W/m-K | 1550 - 1670 BTU-in/hr-ft²-°F | |
MarkeTech W75Cu Tungsten/Copper Heat Sink Material WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c.. |
|||
Thermal Conductivity | 150 - 240 W/m-K | 1040 - 1670 BTU-in/hr-ft²-°F | |
H.C. Starck WCu 70/30 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |