Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 224 - 240 W/m-K | 1550 - 1670 BTU-in/hr-ft²-°F | |
MarkeTech W75Cu Tungsten/Copper Heat Sink Material WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c.. |