Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 24.3 W/m-K @Temperature 20.0 °C |
169 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel CLC 1.2316 Prehardened (300HB) and Corrosion Resistant Mold Steel Description: CLC 1.2316 is a 16%Cr 1% Mo with improved corrosion resistance properties, thanks to the chromium/molybdenum additions. The high cleanliness/homogeneity of the steel makes it specially .. |
|||
Thermal Conductivity | 24.3 W/m-K @Temperature 20.0 °C |
169 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel CLC 1.2316S Prehardened Mold Steel (300HB) with Improved Machinability Description: CLC 1.2316 S grade is a 16%Cr 1%Mo mold steel with improved corrosion resistance properties, thanks to the chromium and molybdenum additions. Furthermore specific sulfur additions are c.. |