Polymer Property : Thermal Conductivity = 23.504 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.00 - 3.3867 W/m-K

@Temperature 50.0 - 100 °C
6.94 - 23.504 BTU-in/hr-ft²-°F

@Temperature 122 - 212 °F
Average value: 2.08 W/m-K Grade Count:15
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..