Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | <= 214 W/m-K | <= 1490 BTU-in/hr-ft²-°F | In-Plane; Angstrom's Method |
GrafTech GRAFCELL® GDB Graphite Gas Diffusion Barrier GRAFCELL® Gas Diffusion Barrier (GDB) material is a thin, perforated structure made from a continuous matrix of expanded natural graphite with excellent electrical conductivity, thermal conductiv.. |