Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 29.8 W/m-K | 207 BTU-in/hr-ft²-°F | |
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 843°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
Thermal Conductivity | 29.8 W/m-K | 207 BTU-in/hr-ft²-°F | |
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.35 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
Thermal Conductivity | 29.8 W/m-K | 207 BTU-in/hr-ft²-°F | |
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.35 mm Strip Heat Treated 843°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
Thermal Conductivity | 29.8 W/m-K | 207 BTU-in/hr-ft²-°F | |
Carpenter Hiperco® Alloy 50 Fe-Co-V Soft Magnetic Alloy, Cold Rolled Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
Thermal Conductivity | 29.8 W/m-K | 207 BTU-in/hr-ft²-°F | |
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |