Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.230 - 0.418 W/m-K | 1.60 - 2.90 BTU-in/hr-ft²-°F | Average value: 0.255 W/m-K Grade Count:16 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |