Polymer Property : Thermal Conductivity = 2.81 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.405 W/m-K
2.81 BTU-in/hr-ft²-°F
ASTM E 1530-11
Quadrant EPP Duratron® PAI T4540 Polyamide-imide, compression molded (ASTM Product Data Sheet)