Polymer Property : Thermal Conductivity = 0.405 W/m-K
Polymer Property :
Thermal Conductivity =
0.405 W/m-K
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Thermal Conductivity
0.405
W/m-K
2.81
BTU-in/hr-ft²-°F
ASTM E 1530-11
Quadrant EPP Duratron® PAI T4540 Polyamide-imide, compression molded (ASTM Product Data Sheet)