Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 2.78 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity >= 2.78 W/m-K
>= 19.3 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® P1011S Electrically Conductive Modified Polyimide
Product Description: EPO-TEK® P1011S is a single component, modified polyimide, high temperature grade, silver-filled electrically and thermally conductive adhesive designed for semiconductor die-a..