Thermal Conductivity 0.200 - 0.340 W/m-K
1.39 - 2.36 BTU-in/hr-ft²-°F
Average value: 0.306 W/m-K Grade Count:25
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..